Excellent quality Multiaxial Creep Testing - RDL-1250W Computer controlled high temperature creep strength testing machine – Chengyu


Specification

Related Video

Feedback (2)

With our loaded encounter and considerate services, we have now been recognized as a trustworthy supplier for lots of worldwide consumers for Low Temperature Mechanical Load Testing Machine, Testing Equipment, Oil Friction Test Machine, Quality is factory's life , Focus on customers' demand is the source of company survival and development, We adhere to honesty and good faith working attitude, looking forward to your coming !
Excellent quality Multiaxial Creep Testing - RDL-1250W Computer controlled high temperature creep strength testing machine – Chengyu Detail:

Application Field

It is mainly used to determine the creep performance and endurance strength of metal materials under a certain temperature and constant load within a specified time.

Implement standard GB/T2039-1997 “Metal Tensile Creep and Endurance Test Method”, JJG276-88 “Verification Regulations for High Temperature Creep and Endurance Strength Testing Machine”.

Key Features

The standard description of the high temperature creep and endurance strength testing machine is used to determine the high temperature creep and endurance strength performance of metal materials under the conditions of constant temperature and constant tensile force in the axial direction of the sample.

Technical Features

Configure the corresponding accessories to achieve:

(1) High temperature endurance strength test:

A. Equipped with high temperature test device and temperature control system,

B. Equipped with permanent pull rod (specimen clamp),

C. The durable strength of the material can be measured under the action of constant temperature and constant tensile load.

(2) High temperature creep test:

A, equipped with high temperature test device and temperature control system,

B, equipped with high temperature creep pull rod (sample fixture)

C, equipped with creep extensometer (deformation drawing device)

D, equipped with creep measuring instrument (deformation measuring instrument).

The creep properties of materials can be measured under constant temperature and constant tensile load.

img (2)

Model

RDL-1250W

Maximum load

50KN

Measuring force range

1%-100%

Test force accuracy grade

0.50%

Displacement accuracy

±0.5%

Speed range

 1*10-5—1*10-1mm/min

Speed accuracy

±0.5%

Effective stretching distance

 200mm

Manually adjustable moving distance

50mm 4mm/revolution

Effective test width

400mm

Sample

round sample φ5×25mm, φ8×40mm


Related Product Guide:

Our eternal pursuits are the attitude of "regard the market, regard the custom, regard the science" plus the theory of "quality the basic, have faith in the main and management the advanced" for Excellent quality Multiaxial Creep Testing - RDL-1250W Computer controlled high temperature creep strength testing machine – Chengyu , The product will supply to all over the world, such as: UAE, Finland, Czech Republic, Due to our strict pursues in quality, and after-sale service, our product gets more and more popular around the world. Many clients came to visit our factory and place orders. And there are also many foreign friends who came for sight seeing, or entrust us to buy other stuff for them. You are most welcome to come to China, to our city and to our factory!
This enterprise in the industry is strong and competitive, advancing with the times and develop sustainable, we are very pleased to have a opportunity to cooperate!
5 Stars By Ina from Sevilla - 2017.01.11 17:15
It can be said that this is a best producer we encountered in China in this industry, we feel lucky to work with so excellent manufacturer.
5 Stars By Rachel from Jeddah - 2018.08.12 12:27
Write your message here and send it to us